How Induction Hardening Works
Principle
When steel is placed inside a copper coil carrying high-frequency current, an alternating magnetic field forms around the coil. The field passes through the steel and induces current inside it, known as eddy current.
Eddy current flows opposite to the coil current. The higher the frequency, the closer the two currents get (the proximity effect), so the eddy current concentrates at the surface of the steel. This is the skin effect. The surface current heats the steel according to Ohm's law, raising its temperature for heat treatment.
Benefits of Induction Hardening
Benefits
Induction hardening uses induced current to heat only the surface areas a part needs, followed by quenching and tempering, so the surface is hard while the core stays tough. The equipment mainly consists of a high-frequency generator, a heating coil and a part-handling fixture. Induction heating is highly efficient, reaching high temperatures in a very short time for a good hardened layer.
A. Selective local hardening, keeping both high hardness and the toughness of the base material
B. Uniform hardness and stable quality
C. Higher fatigue strength
D. Minimal distortion from surface hardening, and straightening is possible when needed
E. Fast heating with minimal oxide scale, keeping precision and improving quality and competitiveness
How Hard Can It Get?
Hardness Reference
Induction hardening reference for steels, shown as material | carbon C% | hardness HRC.
Tool and die steels
・SKH2 high-speed steel | 0.70–0.85 | 62
・SKH3 high-speed steel | 0.70–0.85 | 63
・SKH4A high-speed steel | 0.70–0.85 | 64
・SKH9 high-speed steel | 0.80–0.90 | 63
・SKD1 wear-resistant alloy steel | 2.00–2.20 | 61
・SKD4 premium hot-work die steel | 0.25–0.35 | 50 max
・SKD5 special hot-work die steel | 0.25–0.35 | 50 max
・SKD11 cold-work die steel | 1.40–1.60 | 61
・SKD61 hot-work die steel | 0.35–0.42 | 53 max
・SUJ2 bearing steel | 0.95–1.10 | 60
・SUP3-4 spring steel | 0.95–1.10 | 60
・SKS2 tungsten alloy steel | 1.00–1.10 | 60
・SKS3 die alloy steel | 0.90–1.00 | 60
・SK2-3 carbon tool steel | 1.10–1.30 | 63
・SK5 carbon tool steel | 0.80–0.90 | 60
・S45C medium-carbon steel | 0.42–0.48 | 55–60
Alloy steels
・SCM3-4 Cr-Mo alloy steel | 0.33–0.43 | 58
・SNCM8 Ni-Cr-Mo alloy steel | 0.36–0.43 | 58
・SNC1 Ni-Cr alloy steel | 0.38–0.43 | 50–55
・SNC4 Ni-Cr alloy steel | 0.38–0.43 | 50–55
・SCM21 Cr-Mo alloy steel | 0.13–0.18 | 60
・SNCM21 Ni-Cr-Mo alloy steel | 0.18–0.23 | 60
・S20C, SS41 | induction hardened after carburizing | 60
Cast iron
・Pearlitic malleable iron FMC | 0.35–0.85 | 42–62
・Ductile iron FCD45 | 0.50–0.75 | 48–52
・Gray iron FC30 | 0.45–0.85 | 40–55
・Malleable iron | 0.35–0.90 | 32–63
・Low-alloy cast iron | 0.25–0.85 | 45–63
* Malleable iron: ferrite and pearlite with temper graphite.
* Ductile iron: pearlite with spheroidal graphite, 15–20% ferrite allowed.
* Gray iron: fine pearlite with short flake graphite, 15–20% ferrite allowed.
* Alloy cast iron: pearlite with fine, even graphite plus acicular or network compounds.
Suitable Materials
What Works Best
Medium-carbon steels work best. Common materials:
・Medium-carbon steel: S45C–S50C, including quenched and tempered grades
・Martensitic stainless steel: SUS410, SUS420J1, SUS420J2, SUS440C
・Cr-Mo alloy steel: SAE4135–4140, SCM3–4, SCM435–440
・Ni-Cr-Mo alloy steel: SAE4340, SNCM8, SNCM439
・Bearing steel: SUJ2
・Carbon tool steel: SK2, SK3
Heat Treatment Terms
Key Terms
Quenching
Rapid cooling of steel to form very hard martensite. Three conditions are required: (1) holding the steel in the austenite range for a period (austenitizing); (2) cooling fast enough to avoid pearlite transformation; (3) forming martensite or bainite to harden the steel. Quenching has two stages, heating and cooling, and the quenching temperature depends on the steel.
Tempering
Usually follows quenching. It removes the side effects of quenching while keeping its benefits, stabilizes the structure (tempered martensite), reduces residual stress and improves ductility. Different tempering temperatures give different balances of strength and ductility. Its three goals: adjust hardness after quenching, relieve quenching stress and improve toughness.
Annealing
・Homogenizing (diffusion) annealing: long, high-temperature heating so the chemical composition diffuses evenly.
・Full annealing: hypoeutectoid steel is heated 30–50°C above Ac3 and hypereutectoid steel about 50°C above Ac1, held long enough, then furnace-cooled to soften the steel with the best ductility and a fine grain structure.
・Spheroidizing annealing: turns layered or networked carbides into spheres for better machinability and formability, especially for high-carbon tool steels.
・Soft annealing: heating to 600–650°C (below A1), holding, then air cooling, so work-hardened parts regain toughness for further processing.
・Stress-relief annealing: removes residual stress from forging, casting, machining or welding.
Products & Services
What We Offer
CT10 Fastener Hardening
250+ pcs/min, one-line hardening
CT19 Dual-Disc Machine
Trusted by leading brake makers
Linear Guide Hardening
Precise, low-distortion heating
Custom Induction Systems
Automation built for your line
Custom Induction Coils
Designed per part, patented
Advice & Contract Hardening
Hardening, tempering & brazing
Line Planning & Maintenance
From planning to maintenance
Equipment Planning
Planning concept at a glance
Understanding Induction
Induction basics from our engineers

Request a Quote / Technical Consultation
Tell us about your parts and production volume.
We'll reply within one business day.
+886 939-837-326